9.17. Calculate the amount of each phase present in 1 kg of a 50 wt % Ni-50 wt % Cu alloy at (a) 1400°C, (b) 1300°C, and (c) 1200°C (see Figure 9.9).
Atomic percentage, nickel
10 20 30 40 50 60 70 80 90
°C
1,500 1,455°
1,400 L
1,300 α + L
1,200
1,100 1,084.87°
1,000
α
900
800
700
600
500 Cu 10 20 30 40 50 60 70 80 90 Ni
Weight percentage, nickel